Black Friday: 25% off all winter pieces, no code needed. Shop the sale

Sign in
Journal

How a print run actually works

· The studio

Every design gets printed on a test shirt before it gets printed on yours, which sounds obvious and is the step most shops skip.

The </Dev> tee, straight off the drying rack
The </Dev> tee, straight off the drying rack

What we check

  • That the ink sits in the cotton rather than on top of it
  • That the print survives three washes on the test shirt
  • That the gold reads as gold in daylight, not just under the studio lamp
A print that looks good on the press and cracks in the wash is a print we got wrong.

Run sizes

DesignScreensPieces per run
</Dev>248
404 Not Found236
</> (chest)172

Curing

Water-based ink has to be heat-set or it washes out:

flash dry: 20 seconds
cure: 160°C for 3 minutes
rest: 24 hours before folding

The </Dev> tee and the 404 tee are both printed this way.